Surface analysis
, , , , , and . "Studies of hydrogen-induced degradation processes in Pb(Zr1-xTix)O3 (PZT) and SrBi2Ta2O9 (SBT) ferroelectric film-based capacitors." Integrated Ferroelectrics. Vol. 27. Gordon & Breach Science Publ Inc, Newark, 1999. 147–157.